Role of Si3N4 on microstructure and hardness of hot-pressed ZrB2−SiC composites
By: Zahra Bahararjmand🇹🇷, Mohammad A. Khalilzadeh🇺🇲, Farshad Saberi-Movahed🇺🇲, Tae Hyung Lee🇰🇷, Jinghan Wang🇰🇷, Sea-hoon Lee🇰🇷, Ho Won Jang🇰🇷
SYNTHESIS AND SINTERING 1 (2021) 34–40
#Hot_pressing
#ZrB2_SiC_Si3N4
#Microstructure,
#Hardness
Check it out at https://www.synsint.com/index.php/synsint/article/view/13
By: Zahra Bahararjmand🇹🇷, Mohammad A. Khalilzadeh🇺🇲, Farshad Saberi-Movahed🇺🇲, Tae Hyung Lee🇰🇷, Jinghan Wang🇰🇷, Sea-hoon Lee🇰🇷, Ho Won Jang🇰🇷
SYNTHESIS AND SINTERING 1 (2021) 34–40
#Hot_pressing
#ZrB2_SiC_Si3N4
#Microstructure,
#Hardness
Check it out at https://www.synsint.com/index.php/synsint/article/view/13
Role of Ti3AlC2 MAX phase on characteristics of in-situ synthesized TiAl intermetallics. Part IV: mechanical properties
By: Maryam Akhlaghi🇮🇷, Esmaeil Salahi🇮🇷, Seyed Ali Tayebifard🇮🇷, Gert Schmidt🇩🇪
SYNTHESIS AND SINTERING 2 (2022) 99–104
#SPS
#TiAl_Ti3AlC2
#Flexural_strength
#Hardness
#Fracture_toughness
Check it out at https://doi.org/10.53063/synsint.2022.22103
By: Maryam Akhlaghi🇮🇷, Esmaeil Salahi🇮🇷, Seyed Ali Tayebifard🇮🇷, Gert Schmidt🇩🇪
SYNTHESIS AND SINTERING 2 (2022) 99–104
#SPS
#TiAl_Ti3AlC2
#Flexural_strength
#Hardness
#Fracture_toughness
Check it out at https://doi.org/10.53063/synsint.2022.22103
Role of SPS temperature and holding time on the properties of Ti3AlC2-doped TiAl composites
By: Maryam Akhlaghi🇮🇷, Esmaeil Salahi🇮🇷, Seyed Ali Tayebifard🇮🇷, Gert Schmidt🇩🇪
SYNTHESIS AND SINTERING 2 (2022) 138–145
#TiAl_Ti3AlC2_composites
#Relative_density
#Flexural_strength
#Hardness
#Fracture_toughness
Check it out at https://doi.org/10.53063/synsint.2022.2383
By: Maryam Akhlaghi🇮🇷, Esmaeil Salahi🇮🇷, Seyed Ali Tayebifard🇮🇷, Gert Schmidt🇩🇪
SYNTHESIS AND SINTERING 2 (2022) 138–145
#TiAl_Ti3AlC2_composites
#Relative_density
#Flexural_strength
#Hardness
#Fracture_toughness
Check it out at https://doi.org/10.53063/synsint.2022.2383