https://en.m.wikipedia.org/wiki/Widmanst%C3%A4tten_pattern
> The formation of Ni-poor kamacite proceeds by diffusion of Ni in the solid alloy at temperatures between 450 and 700 °C, and can only take place during very slow cooling, about 100 to 10,000 °C/Myr, with total cooling times of 10 Myr or less. This explains why this structure cannot be reproduced in the laboratory.